KIMYA ABS-R Filament - 750 grams
Kimya ABS-R 3D filament is a standard ABS based on 100% post-consumer recycled material from a recycling company based
in France. Its use contributes to the development of a circular economy by reducing the emission of C02, the
consumption of water and electricity as well as the oil resources necessary for its production. Acrylonitrile
butadiene styrene (ABS) is a thermoplastic polymer combining lightness, high impact resistance and good temperature
resistance. ABS is suitable for functional prototyping, enclosure applications in industries such as appliances,
telephony, automotive, hardware and toys.
- Better heat resistance than PLA (around 90°C)
- Good impact resistance
- Made from 100% post-consumer recycled ABS – reduced environmental impact
- Compliant with REACH regulation and RoHS directive
2-year KIMYA warranty.
Store away from light, humidity and heat to maintain the properties of the product.
FILAMENT PROPERTIES
PROPERTIES |
TEST METHODS |
VALUES |
Diameter |
INS-6712 |
1.75 ± 0.1 mm 2.85 ± 0.1 mm |
Density |
ISO 1183-1 |
1.049 g/cm3 |
Moisture rate |
INS-6711 |
< 0.5% |
Melt flow index (MFI) |
ISO 1133-1 (@210°C – 2,16 kg) |
14.2 g/10min |
Glass transition temperature (Tg) |
ISO 11357-1 DSC (10°C/min - 20-220°C) |
110 °C |
PRINT PARAMETERS AND SPECIMENS DIMENSIONS
PRINTING DIRECTION |
XY |
Printing Speed |
20-50 mm/s |
Infill |
100% - rectilinear |
Infill Angle |
45°/-45° |
Nozzle Temperature |
190-210°C |
Bed T° |
20-60°C |
PRINTED SPECIMENS PROPERTIES
|
PROPERTIES |
TEST METHODS |
VALUES |
MECHANICAL PROPERTIES
|
Tensile modulus |
ISO 527-2/5A/50 |
1,722 MPa |
Tensile Strength |
ISO 527-2/5A/50 |
32.2 MPa |
Tensile strain at strength |
ISO 527-2/5A/50 |
2.1 % |
Tensile Stress at Break |
ISO 527-2/5A/50 |
27.5 MPa |
Tensile strain at break (type A) |
ISO 527-2/5A/50 |
9.4 % |
Flexural modulus |
ISO 178 |
1,557 MPa |
Flexural stress at conventional deflection (3,5% strain)*
|
ISO 178 |
48.4 MPa |
Charpy impact resistance |
ISO 179-1/1eA |
8.5 kJ/m² |
Shore Hardness |
ISO 868 |
72.2D |
Note 1 |
*According to ISO 178, end of the test at 5% deformation even if there
is no specimen break.
|
Note 2 |
The data should be considered as indicative values - Properties can be
influenced by production conditions.
|
PRINT SETTINGS:
- PRINT SPEED: 20-60 mm/s
- EXTRUSION TEMPERATURE: 250-270°C
- PLATFORM TEMPERATURE : 90-110°C
- CHAMBER TEMPERATURE : 20-80°C
MISCELLANEOUS
Spool Material |
PC |
Steaming Temperature |
80°C |
Steaming Duration |
2h-4h |
CERTIFICATION AND USES
PROPERTIES |
RATING |
Ease to print |
|
Rigidity |
|
Elasticity |
|
Impact Strength |
|
Temperature Resistance |
|
Weather Resistance |
|
RoHs |
Compliant |
EU 10/2011 |
Non Compliant |
FDA |
Non Compliant |
UL94 - V0 |
Non Compliant |
ESD Protection |
Non Compliant |