KIMYA ABS-R Filament - 750 grams

Kimya ABS-R 3D filament is a standard ABS based on 100% post-consumer recycled material from a recycling company based in France. Its use contributes to the development of a circular economy by reducing the emission of C02, the consumption of water and electricity as well as the oil resources necessary for its production. Acrylonitrile butadiene styrene (ABS) is a thermoplastic polymer combining lightness, high impact resistance and good temperature resistance. ABS is suitable for functional prototyping, enclosure applications in industries such as appliances, telephony, automotive, hardware and toys.

  • Better heat resistance than PLA (around 90°C)
  • Good impact resistance
  • Made from 100% post-consumer recycled ABS – reduced environmental impact
  • Compliant with REACH regulation and RoHS directive

2-year KIMYA warranty.
Store away from light, humidity and heat to maintain the properties of the product.

FILAMENT PROPERTIES

PROPERTIES TEST METHODS VALUES
Diameter INS-6712 1.75 ± 0.1 mm
2.85 ± 0.1 mm
Density ISO 1183-1 1.049 g/cm3
Moisture rate INS-6711 < 0.5%
Melt flow index (MFI) ISO 1133-1 (@210°C – 2,16 kg) 14.2 g/10min
Glass transition temperature (Tg) ISO 11357-1 DSC (10°C/min - 20-220°C) 110 °C

PRINT PARAMETERS AND SPECIMENS DIMENSIONS

PRINTING DIRECTION XY
Printing Speed 20-50 mm/s
Infill 100% - rectilinear
Infill Angle 45°/-45°
Nozzle Temperature 190-210°C
Bed T° 20-60°C

PRINTED SPECIMENS PROPERTIES

PROPERTIES TEST METHODS VALUES
MECHANICAL
PROPERTIES
Tensile modulus ISO 527-2/5A/50 1,722 MPa
Tensile Strength ISO 527-2/5A/50 32.2 MPa
Tensile strain at strength ISO 527-2/5A/50 2.1 %
Tensile Stress at Break ISO 527-2/5A/50 27.5 MPa
Tensile strain at break (type A) ISO 527-2/5A/50 9.4 %
Flexural modulus ISO 178 1,557 MPa
Flexural stress at conventional deflection (3,5% strain)* ISO 178 48.4 MPa
Charpy impact resistance ISO 179-1/1eA 8.5 kJ/m²
Shore Hardness ISO 868 72.2D
Note 1 *According to ISO 178, end of the test at 5% deformation even if there is no specimen break.
Note 2 The data should be considered as indicative values - Properties can be influenced by production conditions.

PRINT SETTINGS:

  • PRINT SPEED: 20-60 mm/s
  • EXTRUSION TEMPERATURE: 250-270°C
  • PLATFORM TEMPERATURE : 90-110°C
  • CHAMBER TEMPERATURE : 20-80°C

MISCELLANEOUS

Spool Material PC
Steaming Temperature 80°C
Steaming Duration 2h-4h

CERTIFICATION AND USES

PROPERTIES RATING
Ease to print
Rigidity
Elasticity
Impact Strength
Temperature Resistance
Weather Resistance
RoHs Compliant
EU 10/2011 Non Compliant
FDA Non Compliant
UL94 - V0 Non Compliant
ESD Protection Non Compliant
Go to full site